Knife-Coated Flex Banner Fabric

Premium knife-coated PVC banner fabric with an ultra-smooth print surface and excellent dimensional stability for large-format digital printing.

Specifications

Weight (g/m²) 440–610 g/m²
Width (m) Up to 3.20 m
Thickness (mm) 0.35–0.55 mm
Color White
Material Knife-coated PVC on high-tenacity yarn
Tensile Strength (N/5cm) ≥ 1000 N/5cm
Tear Strength (N) ≥ 80 N
Adhesion Strength (N/5cm) ≥ 45 N/5cm
Flame Retardancy Standard Optional
Send Inquiry

Product Details

Product Introduction

Our knife-coated flex banner fabric is produced through a precision knife-coating process that delivers an exceptionally smooth, uniform print surface. It is the preferred choice for high-end large-format printing where fine detail and vivid color matter.

Product Features

  • Ultra-smooth knife-coated surface for fine detail
  • Excellent ink adhesion and color vibrancy
  • High dimensional stability — no stretching during printing
  • Good flexibility for easy handling and installation
  • Suitable for solvent and UV digital printing
  • Anti-scratch surface protection

Product Applications

  • Large-format digital printing
  • Premium banners and posters
  • Indoor and outdoor advertising
  • Retail and exhibition displays
  • Photo-quality large graphics